You could go with some weld-on 4 mixed with 16, it will be a little thicker, but still be a good flowing liquid. You could also run 16 on the inside, then 4 on the outside after the 16 has cured. HTH
Ram
You could go with some weld-on 4 mixed with 16, it will be a little thicker, but still be a good flowing liquid. You could also run 16 on the inside, then 4 on the outside after the 16 has cured. HTH
Ram