Originally Posted by
txav8r
Weldon 16 contracts too much when it dries. You will get air bubbles under the seam if you apply too much.
Like Jose said, try weld on 4. you can get it at any of the plastic places here in town. I think there are 3 of them.
Very true Jack. I used excess #16 on an acrylic patch and it contracted, split some of the plastic, and caused little fissures to appear all over the place.
That being said, I still have an extra tube of #16 of you'd like it.
I refuse to join any club that would have me as a member.